Stellite coating is done either
by TIG Process or Metallizing Process and the hardness of
the coated Surface will be 45-50 RC. It has high corrosion
and abrasion resistance at high temperatures.
Tungsten Carbide coating is done
by Metallizing Process and the hardness of the coated Surface
will be minimum 60 RC. It got high Abrasion Resistance at
lower temperatures.
TEMP TECH Tech also manufactures
Thermowells with Teflon coating for Corrosion Resistance
at low temperatures.
Applications: - Coal Blast Mills, Ash handling plants,
Corrosive Media